Factory For China Sintered Neodymium/ Ferrite/ SmCo Magnet Mini Magnet

Request a Quote

Products Details

Our organization aims to operating faithfully, serving to all of our consumers , and working in new technology and new machine continually for Factory For China Sintered Neodymium/ Ferrite/ SmCo Magnet Mini Magnet, We welcome you to definitely be a part of us during this path of making a affluent and productive business enterprise together. Our organization aims to operating faithfully, serving to all of our consumers , and working in new technology and new machine continually for China Mini Magnet, Micro Magnetic, We've customers from more than 20 countries and our reputation has been recognized by our esteemed customers. Never-ending improvement and striving for 0% deficiency are our two main quality policies. Ought to you want anything, don't hesitate to contact us. Introduction: Hard ferrites based on barium ferrite and strontium powders (chemical formula BaO • 6Fe2O3 and SrO • 6Fe2O3) manufactured. They consist of oxidized metals, thus included in the ceramic materials group. They consist of approx. 90% iron oxide (Fe2O3) and 10% alkaline earth oxide (BaO or SrO) – raw materials which are plentiful and inexpensive. They divide into isotropic and anisotropic, the particles of the latter are aligned in a single direction which obtaining better magnetic characteristics. Isotropic magnets are shaped by compressing while anisotropic magnets are compressed within a magnetic field. This provides the magnet with a preferential direction and triples its energy density. Advantage: As is typical of oxide ceramics, hard ferrite magnets display relatively resistant behavior towards moisture, solvents, alkaline solutions, weak acids, salts, lubricants and gas pollutants. Generally, hard ferrite magnets can therefore be used without additional corrosion protection. Feature: Due to their great hardness (6-7 Mohs), Ferrite magnets are brittle and sensitive to knocks or bending. During processing, they have to be machined with diamond tools. Operating temperatures with ferrite magnets are generally between –40ºC and 250ºC. Application: Different shapes are used in utomotive engineering, such as automation and measurement control. Other applications such as Automobile electrical machinery (wipers, sit chair motor), Teaching, Door absorber, Magnetic bike and massage chair, etc. Today, hard ferrites represent the largest proportion of permanent magnets produced. In contrast to AlNiCo magnets, hard ferrites are characterized by flux densities but high coercive field strengths. This results in the generally flat shape of the materials. Barium ferrite and strontium ferrite are differentiated depending on the starting material. All stated values were determined using standard samples according IEC 60404-5. The following specifications serve as reference values and may differ. Sintered Ferrite Magnet Physical Properties Grade Remanence Rev. Temp.   Coeff. Of Br Coercive Force Intrinsic Coercive Force Rev. Temp.-Coeff. Of Hcj Max. Energy Product Max. Operating Temperature Density Br (KGs) Hcb (KOe) Hcj (KOe) (BH)max. (MGOe) g/cm³ Y10T 2.0-2.35 -0.20 1.57-2.01 2.64-3.52 +0.30 0.8-1.2 250℃ 4.95 Y20 3.2-3.8 -0.20 1.70-2.38 1.76-2.45 +0.30 2.3-2.8 250℃ 4.95 Y22H 3.1-3.6 -0.20 2.77-3.14 3.52-4.02 +0.30 2.5-3.2 250℃ 4.95 Y23 3.2-3.7 -0.20 2.14-2.38 2.39-2.89 +0.30 2.5-3.2 250℃ 4.95 Y25 3.6-4.0 -0.20 1.70-2.14 1.76-2.51 +0.30 2.8-3.5 250℃ 4.95 Y26H 3.6-3.9 -0.20 2.77-3.14 2.83-3.21 +0.30 2.9-3.5 250℃ 4.95 Y27H 3.7-4.0 -0.20 2.58-3.14 2.64-3.21 +0.30 3.1-3.7 250℃ 4.95 Y28 3.7-4.0 -0.20 2.20-2.64 2.26-2.77 +0.30 3.3-3.8 250℃ 4.95 Y30 3.7-4.0 -0.20 2.20-2.64 2.64-2.77 +0.30 3.3-3.8 250℃ 4.95 Y30H-1 3.8-4.0 -0.20 2.89-3.46 2.95-3.65 +0.30 3.4-4.1 250℃ 4.95 Y30BH 3.8-3.9 -0.20 2.80-2.95 2.90-3.08 +0.30 3.4-3.7 250℃ 4.95 Y30-1 3.6-4.0 -0.20 1.70-2.14 1.76-2.51 +0.30 2.8-3.5 250℃ 4.95 Y30BH-1 3.8-4.0 -0.20 2.89-3.46 2.95-3.65 +0.30 3.4-4.0 250℃ 4.95 Y30H-2 3.95-4.15 -0.20 3.46-3.77 3.90-4.21 +0.30 3.5-4.0 250℃ 4.95 Y20-2 3.95-4.15 -0.20 3.46-3.77 3.90-4.21 +0.30 3.5-4.0 250℃ 4.95 Y32 4.0-4.2 -0.20 2.01-2.38 2.07-2.45 +0.30 3.8-4.2 250℃ 4.95 Y33 4.1-4.3 -0.20 2.77-3.14 2.83-3.21 +0.30 4.0-4.4 250℃ 4.95 Y35 4.0-4.1 -0.20 2.20-2.45 2.26-2.51 +0.30 3.8-4.0 250℃ 4.95 Note: · We remain the same as above unless specified from customer. Curie temperature and temperature coefficient are for reference only, not as a basis for decision. · The maximum working temperature of magnet is changeable due to ratio of length and diameter and environment factors.

contact us

Please feel free to give your inquiry in the form below We will reply you in 24 hours

Leave YourMessage

Thank you! We will reply you via email within 24 hours.

return