SmCo Magnet

Request a Quote

Products Details

Sintered SmCo Magnet Physical Properties Material Grade Remanence Rev. Temp.- Coeff. Of Br Coercive Force Intrinsic Coercive Force Rev. Temp.-Coeff. Of Hcj Max. Energy Product Max. Operating Temperature Density Br (KGs) Hcb (KOe) Hcj (KOe) (BH)max. (MGOe) g/cm³ SmCo5 XG16 8.1-8.5 -0.050 7.8-8.3 15-23 -0.30 14-16 250℃ 8.3 XG18 8.5-9.0 -0.050 8.3-8.8 15-23 -0.30 16-18 250℃ 8.3 XG20 9.0-9.4 -0.050 8.5-9.1 15-23 -0.30 19-21 250℃ 8.3 XG22 9.2-9.6 -0.050 8.9-9.4 15-23 -0.30 20-22 250℃ 8.3 XG24 9.6-10.0 -0.050 9.2-9.7 15-23 -0.30 22-24 250℃ 8.3 XG16S 7.9-8.4 -0.050 7.7-8.3 ≥23 -0.28 15-17 250℃ 8.3 XG18S 8.4-8.9 -0.050 8.1-8.7 ≥23 -0.28 17-19 250℃ 8.3 XG20S 8.9-9.3 -0.050 8.6-9.2 ≥23 -0.28 19-21 250℃ 8.3 XG22S 9.2-9.6 -0.050 8.9-9.5 ≥23 -0.28 21-23 250℃ 8.3 XG24S 9.6-10.0 -0.050 9.3-9.9 ≥23 -0.28 23-25 250℃ 8.3 Sm2Co17 XG24H 9.5-10.2 -0.025 8.7-9.6 ≥25 -0.20 22-24 350℃ 8.3 XG26H 10.2-10.5 -0.030 9.4-10.0 ≥25 -0.20 24-26 350℃ 8.3 XG28H 10.3-10.8 -0.035 9.5-10.2 ≥25 -0.20 26-28 350℃ 8.3 XG30H 10.8-11.0 -0.035 9.9-10.5 ≥25 -0.20 28-30 350℃ 8.3 XG32H 11.0-11.3 -0.035 10.2-10.8 ≥25 -0.20 29-32 350℃ 8.3 XG22 9.3-9.7 -0.020 8.5-9.3 ≥18 -0.20 20-23 300℃ 8.3 XG24 9.5-10.2 -0.025 8.7-9.6 ≥18 -0.20 22-24 300℃ 8.3 XG26 10.2-10.5 -0.030 9.4-10.0 ≥18 -0.20 24-26 300℃ 8.3 XG28 10.3-10.8 -0.035 9.5-10.2 ≥18 -0.20 26-28 300℃ 8.3 XG30 10.8-11.0 -0.035 9.9-10.5 ≥18 -0.20 28-30 300℃ 8.3 XG32 11.0-11.3 -0.035 10.2-10.8 ≥18 -0.20 29-32 300℃ 8.3 XG26M 10.2-10.5 -0.035 8.5-9.8 12-18 -0.20 24-26 300℃ 8.3 XG28M 10.3-10.8 -0.035 8.5-10.0 12-18 -0.20 26-28 300℃ 8.3 XG30M 10.8-11.0 -0.035 8.5-10.5 12-18 -0.20 28-30 300℃ 8.3 XG32M 11.0-11.3 -0.035 8.5-10.7 12-18 -0.20 29-32 300℃ 8.3 XG24L 9.5-10.2 -0.025 6.8-9.0 8-12 -0.20 22-24 250℃ 8.3 XG26L 10.2-10.5 -0.035 6.8-9.4 8-12 -0.20 24-26 250℃ 8.3 XG28L 10.3-10.8 -0.035 6.8-9.6 8-12 -0.20 26-28 250℃ 8.3 XG30L 10.8-11.5 -0.035 6.8-10.0 8-12 -0.20 28-30 250℃ 8.3 XG32L 11.0-11.5 -0.035 6.8-10.2 8-12 -0.20 29-32 250℃ 8.3  Note: · We remain the same as above unless specified from customer. Curie temperature and temperature coefficient are for reference only, not as a basis for decision.· The maximum working temperature of magnet is changeable due  to ratio of length and diameter and environment factors.   Advantage: Use of these magnets is conditioned by the temperature in a wide range running from 250ºC to 350ºC and their Curie temperature can be as high as 710 to 880 °C.  Therefore, SmCo magnet has the best magnetic stability due to the superior resistance to high temperature. SmCo magnets are characterized by very high corrosion resistance, no coating required for surface protection.   Feature: A disadvantage of SmCo magnets is the marked brittleness of the material – a factor which must be particularly taken into account during processing. The magnets are galvanized or coated by  cathodic electrodeposition for certain applications.   Application: In areas high operating temperature, high corrosion and oxidation resistance are crucial. Such as, Electronic magnetron, Magnetic transmission, Magnetic treatment, Magnistor, etc. All stated values were determined using standard samples according IEC 60404-5. The following specifications serve as reference values and may differ. The max. operating temperature is dependent on the magnet dimesion and the specific application. For more information please contact our application engineers.    

contact us

Please feel free to give your inquiry in the form below We will reply you in 24 hours

Leave YourMessage

Thank you! We will reply you via email within 24 hours.

return